Development and verification of microstructure, residual stress and deformation simulation capability for additive free-form deposition using multiple superalloys - JTI-CS2-2018-CfP08-ENG-02-09
Deadline: 12 Jul 2018   CALL EXPIRED

EU logo mono EC - Horizon 2020

 Innovation
 Aeronautics Industries
 Horizon2020
 Research

Specific Challenge:

Development and verification of microstructure, residual stress and deformation simulation capability for additive free-form powder deposition using multiple superalloys. The methods should be capable of handling typical design features for engine structures with a turn-around time for simulation set-up, execution and evaluation within a working week. Validation experiments using the laser blown powder process are to be performed by the CfP consortium on design features. Please refer to the full topic descriptions document published in this call.